Problem, idea and solution
-
Problem
The double dovetail guiding of a milling machine was completely worn.
-
Solution
Revamo has repaired the guiding by milling the worn out of the carriages and thermal spaying of the stationary guiding. Afterwarts the coating has been milled to the right fit.
-
Abrasive wear
Wear deformation caused by surfaces or particles rubbing on one another. The abrasive is made up of a hard and/or sharp...
-
Dimensional recovery
Every type of wear requires dimensional recovery. Dimensional recovery is also required when a design or machining error...
Specifications
Principle dimensions (LxWxH): 1.500x600x300mm | Base material: 0.6025 (GG25) | Coating: Bronze |