Problem, idea and solution
-
Problem
This is a drive roller of a conveyor belt which runs in liquid. The lifetime of the roller coating is to short and the friction is insufficient.
-
Solution
Revamo has spayed a grip / wear layer. Afterwards the layer is minimal machined in order to achieve the right roughness.
-
Abrasive wear
Wear deformation caused by surfaces or particles rubbing on one another. The abrasive is made up of a hard and/or sharp...
-
Chemical attack
A type of wear that occurs as a result of an (electro)chemical reaction between the component and the surrounding...
Specifications
Principle dimensions (LxWxH): Ø600x5.520mm | Base material: 1.4301 (Aisi 304) | Coating: WcCoCr |