Problem, idea and solution
-
Problem
The piston of a sand press for a foundry is badly worn out. The sand has dug in grooves of up to 2.5 mm.
-
Solution
Revamo repaired the piston by flame spraying and grinding.
-
Abrasive wear
Wear deformation caused by surfaces or particles rubbing on one another. The abrasive is made up of a hard and/or sharp...
-
Dimensional recovery
Every type of wear requires dimensional recovery. Dimensional recovery is also required when a design or machining error...
Specifications
Principle dimensions (LxWxH): Ø450x558mm | Base material: 0.6025 (GG25) | Coating: Chrome steel |