Problem, idea and solution
-
Problem
Of these crankshaft (Leopard tank) a sealing position is worn.
-
Solution
Revamo repaired this crankshaft by flame spraying and grinding. Revamo is able to do a complete revision of a crankshaft.
-
Abrasive wear
Wear deformation caused by surfaces or particles rubbing on one another. The abrasive is made up of a hard and/or sharp...
-
Dimensional recovery
Every type of wear requires dimensional recovery. Dimensional recovery is also required when a design or machining error...
Specifications
Principle dimensions (LxWxH): Ø350x1.600mm | Base material: 1.6582 (34CrNiMo6) | Coating: Chrome steel |