Problem, idea and solution
- 
					 
					ProblemThese disks rotate in an abrasive and corrosive environment. The discs are fully tailor-made, and still need to be welded to an axle. 
- 
					 
					SolutionThe discs are coated with Stellite. 
 Because flame spraying is a "cold" process, the component does not deform, and the fittings remain intact.
 The discs are coated by the robot.
 
- 
					 
					Abrasive wearWear deformation caused by surfaces or particles rubbing on one another. The abrasive is made up of a hard and/or sharp... 
- 
					 
					Chemical attackA type of wear that occurs as a result of an (electro)chemical reaction between the component and the surrounding... 
Specifications
| Principle dimensions (LxWxH): Ø630x170mm | Base material: 1.4404 (Aisi 316) | Coating: Stelliet | 